学术成果 |
[1] Chaohui Guo,Weiwei Zhu*, Yuanxun Shen, Yaodong Liu, Xu Ran*, Joining ZTA ceramics by using Dy2O3-Al2O3-SiO2 glass ceramic filler,Journal of European Ceramic Society, 2020, 40: 5819-5828. (SCI, IF=4.495) [2] Weiwei Zhu*,He Zhang, Dahui Xue, Haifeng Jiang, Xu Ran, Joining alumina ceramic by using glass ceramic filler with high crystallinity for high temperature application,Ceramics International, 2019, 45: 20999-21003. (SCI, IF=3.83) [3] He Zhang,Weiwei Zhu*, Teng Zhang, Chaohui Guo, Xu Ran, Effect of brazing temperature on microstructure and mechanical property of high nitrogen austenitic stainless steel joints brazed with Ni-Cr-P filler, ISIJ International, 2019, 59: 300-304. (SCI, IF=1.405) [4]Weiwei Zhu*,He Zhang,Chaohui Guo,Yaodong Liu,Xu Ran*, Wetting and brazing characteristic of high nitrogen austenitic stainless steel and 316L austenitic stainless steel by Ag-Cu filler,Vacuum, 2019, 166: 97-106. (SCI, IF=2.906) [5] Haohao, Zou,Weiwei Zhu*, Ying Han, Siqi Zhan, Xu Ran*, Effect of CrFeC alloy particles on the tribological behavior of copper-graphite-silica composites,Materials Research Express, 2019, 11: 116542 (SCI, IF=1.929) [6] Weiwei Zhu*, Haifeng Jiang, He Zhang, Suqiu Jia, Yaodong Liu, Effect of TiO2 and CaF2 on the crystallization behavior of Y2O3-Al2O3-SiO2 glass ceramics,Ceramics International, 2018, 44 (6): 6653-6658. (SCI, IF=3.83) [7] Weiwei Zhu*, Haifeng Jiang, Shicheng Sun, Suqiu Jia, Yaodong Liu, Effect of TiO2 content on the crystallization behavior and properties of CaO-Al2O3-SiO2 glass ceramic fillers for high temperature joining application,Journal of Alloys and Compounds, 2018, 732 (25): 141-148. (SCI, IF=4.65) [8]Weiwei Zhu*, Haifeng Jiang, He Zhang, Shicheng Sun, Yaodong Liu, Microstructure and strength of high nitrogen steel joints brazed with Ni-Cr-B-Si filler,Materials Science and Technology, 2018, 34(8): 926-933. (SCI, IF=1.835) [9] Haohao Zou, Xu Ran*,Weiwei Zhu*, Yong Wang, Siqi Zhan, Zhikang Hao,Tribological behavior of copper-graphite composites reinforced with Cu-coated or uncoated SiO2 particles.Materials, 2018, 11, 2414. (SCI, IF=3.057) [10] Bowei Luo, Shenglin Jiang,Weiwei Zhu, Youyou Hu, Yingxiong Qin, Xiahui Tang, Laser joining of Al2O3 liners with Al2O3-MgO-SiO2 glass ceramic fillers,Journal of Materials Processing Technology, 2018, 260: 48-56. (SCI, IF=4.669) [11]朱巍巍*,陈继春,微晶玻璃焊料在连接过程中的晶化行为研究,无机材料学报, 2015, 30(12): 1310-1314. (SCI, IF=0.901) [12]Weiwei Zhu, Jichun Chen, Chunhai Jiang, Chuanyong Hao, Jinsong Zhang*, Effects of Ti thickness on microstructure and mechanical properties of alumina-Kovar joints brazed with Ag-Pd/Ti filler,Ceramics International, 2014, 40(4): 5699-5705. (SCI, IF=3.83) [13]Weiwei Zhu, Jichun Chen, Chuanyong Hao, Jinsong Zhang*, Microstructure and strength of Al2O3/Al2O3 joints bonded with ZnO-Al2O3-B2O3-SiO2 glass-ceramic,Journal of Materials Science & Technology, 2014, 30(9): 944-948. (SCI, IF=6.155) [14]Weiwei Zhu, Jichun Chen, Chunhai Jiang, Chuanyong Hao, Jinsong Zhang*, Joining of porous alumina with a CaO-Al2O3-SiO2 glass-ceramic,Journal of the American Ceramic Society, 2013, 96(6): 1738-11744. (SCI, IF=3.502) [15]朱巍巍,姜海峰,崔佳,刘耀东,一种陶瓷内衬复合钢管的连接方法,2018.12.14,中国,ZL201611070044.7 |